PLATE TYPE |
ASA / ISO |
DEVELOPER |
DILUTION |
TEMP |
DEV TIME |
NOTES |
---|---|---|---|---|---|---|
STANDARD PLATES |
2 |
510 PYRO |
1+150 |
20°C |
5min |
|
STANDARD PLATES |
2 |
FOMATOL LQN |
1+59 |
20°C |
4min |
|
STANDARD PLATES |
2 |
KODAK T-Max |
1+8 |
20°C |
2min |
/ |
STANDARD PLATES |
2 |
KODAK HC-110 / Ilfotec HC |
1+31 |
20°C |
5min |
/ |
STANDARD PLATES |
2 |
D76/ID-11 |
STOCK |
20°C |
3min |
|
STANDARD PLATES |
2 |
Moersch ECO 4812 |
1+30 |
20°C |
3min |
|
STANDARD PLATES |
2 |
Rodinal |
1+50 |
20°C |
4min |
/ |
STANDARD PLATES |
2 |
Dektol |
STOCK |
20°C |
5min |
/ |
STANDARD PLATES |
2 |
Bellini Euro HC |
1+31 |
20°C |
5min |
/ |
STANDARD PLATES |
2 |
XTOL |
1+33 |
20°C |
7min |
/ |
STANDARD PLATES |
2 |
D23 |
STOCK |
20°C |
9min |
/ |
STANDARD PLATES |
2 |
Cinestill DF96 monobath |
STOCK |
20°C |
8min |
/ |
STANDARD PLATES |
2 |
CAFFENOL |
In the video |
20°C |
4-5min |
DEVELOPING CHART FOR PROCESSING ZEBRA DRY PLATE TINTYPES & AMBROTYPES
(on mobile tilt your phone to the side or swipe left to reveal all the info)
PLATE TYPE |
ASA / ISO |
DEVELOPER |
DILUTION |
TEMP |
DEV TIME |
NOTES |
---|---|---|---|---|---|---|
STANDARD PLATES |
2 |
510 PYRO |
1+59 |
20°C |
3min |
|
STANDARD PLATES |
2 |
FOMATOL LQN |
1+150 |
20°C |
4-5min |
|
STANDARD PLATES |
2 |
KODAK T-Max |
STOCK |
20°C |
2min |
|
STANDARD PLATES |
2 |
D76/ID-11 |
STOCK |
20°C |
2min |
|
STANDARD PLATES |
2 |
KODAK HC-110 |
1+59 |
20°C |
3min30s |
/ |
STANDARD PLATES |
2 |
Moersch ECO 4812 |
1+30 |
20°C |
2min |
|
STANDARD PLATES |
2 |
Dektol |
STOCK |
20°C |
3min |
/ |
STANDARD PLATES |
2 |
Bellini Euro HC |
1+33 |
20°C |
3min30s |
/ |
PROCESSING TIMES FOR FIXERS
FIXER |
DILUTION |
TEMP. |
FIXING TIME |
NOTES |
---|---|---|---|---|
FOMA FOMAFIX |
1:4 |
20°C |
3min |
|
ECO Zonefix |
stock |
20°C |
2min |
|
Ilford Rapid Fix |
1:4 |
20°C |
5min |